"Masterbond" does a food grade epoxy coating, that also has good high temperature properties. 

EP42HT-2FG


As long as you coat the "working surfaces" of the mold with something like this, you should have no problems making the "mold" itself from "standard resins and reinforcement.

You state that you need to use the mold in a press, that probably means that you will have to add some sort of reinforcement to the resin.

This could be either in the form of standard "cloth" CF or glassfibre, or you could use powdered CF...

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 12 Years Ago by Dravis
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
dont realy know what you are making, but thought about a food grade silicone? 

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




stan0102
stan0102
Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)Junior Member (11 reputation)
Group: Forum Members
Posts: 1, Visits: 5
Hi everyone,
I want to make a food grade resin mould for making pie crusts. I know how to make the mould, avoiding undercuts etc, but cannot find any information on what materials to use.
A pourable resin would be ideal. The mould would be placed in a press and only be in contact with the dough for less than 5 seconds.
Any ideas would be gratefully received.
Regards,
John.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search