Just use a lint free cloth as the shrink tape goes on and is shrunk. You will get excess squeezed out the ends and along the tape. Wiping it off will aid removal of the tape once the repair has cured.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|