Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Unfortunately i can't combine the threads.
2 to 3 wraps is generally enough but it depends on the wall thickness and severety of damage. The top thin tubes usually 2 is sufficient maybe 3 if its a complete break. The thicker sections may need more layers to replace the strength but generally tend to break less.
If your kit has the wrong cloth in it then you can either send back the roll with a note including order number and we will ensure the right material is sent, or give us a call or email and we can fix it that way. User accounts on the forum are not linked to customer accounts on the webshop so I cannot see your order from here.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|