Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
How to make a split mould for this spoiler? 2 piece, 3 piece?
How to make a split mould for this spoiler? 2 piece, 3 piece?
Post Reply
Like
3
1
2
Next
Jump To Page
How to make a split mould for this spoiler? 2 piece, 3 piece?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Bonobo
Bonobo
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
Can anyone give me some advice as to how to make a mould from this spoiler plug I'm making?
Here's an illustration of the profile to show the detail
I'm thinking a split along the top and barriers to the front and rear edges?
Reply
Like
3
ajb100
ajb100
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
For ease I would go with a three piece mould although you probably wouldn't have any issues with a two piece mould
Reply
Like
2
andygtt
andygtt
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 157,
Visits: 1.2K
do you intend to make it with all 3 sides and thus bond them together, or do you want to try to make it 1 piece as this will effect how I would make the mould?
personally Id make it 2 piece and have one of the joins under the part that bolts to the car (i.e. hidden face) and the other on an edge, but leave a gap in the hidden edge (so it won't be a complete 3 sided totally joined piece, but does it need to be? would 2 sides with returns to bolt to car be ok?)... I would then lay the 2 parts up with the first layer, then bolt them together and fully overlay the back edges for strength, then bag it up.
Reply
Like
2
Bonobo
Bonobo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
Do you mean something liike this?
Reply
Like
2
Bonobo
Bonobo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
Can anyone help me please?
Would i need a 3 / 4 piece mould like this in order to release the part?
Reply
Like
3
FLD
FLD
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
Why not have the base as one part (joins front and back) and the main body as the second part. Joints would be virtually hidden and it shouldn't mecahnically lock.
My paint skills are nowhere near as good as yours so I hope the description is OK!
Reply
Like
3
Bonobo
Bonobo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
FLD (17/07/2014)
Why not have the base as one part (joins front and back) and the main body as the second part. Joints would be virtually hidden and it shouldn't mecahnically lock.
My paint skills are nowhere near as good as yours so I hope the description is OK!
But wouldn't it then be a closed mould? How would I lay it up and bag it?
Or do you mean make the top and bottom pieces separately and bond them together after.
Edited
11 Years Ago by
Bonobo
Reply
Like
3
FLD
FLD
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
Yeah, I'd do them as separate parts. 3mm soric core will leave you with a nice large bonding surface
Reply
Like
3
Bonobo
Bonobo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 85,
Visits: 1.2K
Like this? top pic shows both moulds with lay up,bottom pic shows both parts trimmed ready to be bonded
Reply
Like
3
FLD
FLD
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
Thats the one, exactly what I was meaning. I'm a belt and braces man so I'd put tape down the inside too.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
1
2
Next
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search