I have made most of my body panels and would like to paint the carbon .

There is no gelcoat just infused resin finish

Is there a special way I have to prime this for painting ???

Any info would be good on painting these panels

Im using two pack paint,,

Thanks Daz.
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
As you would normal car

We hit with 800 an that's it
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
Cheers Rob ,

I thought I may need some special primer,,
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
I find that with any composite panel its best to use a plastic primer or adhesion promotor before using an opaque proper primer.  Its just a dust coat to help it stick.  If your panels are REALLY flexible then you can add a flex additive to two pack.  I used this for lacquering EF80 but you shouldn't need it for normal panels.
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
cheers
20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
I have found that with an infused(no gel or surface coat) part even the slightest amount of sanding with 800 will start to expose fibres, .... doesn't this hurt the adhesion of the paint to the part?