Group: Forum Members
Posts: 468,
Visits: 2.7K
|
I find that with any composite panel its best to use a plastic primer or adhesion promotor before using an opaque proper primer. Its just a dust coat to help it stick. If your panels are REALLY flexible then you can add a flex additive to two pack. I used this for lacquering EF80 but you shouldn't need it for normal panels.
|