I have made most of my body panels and would like to paint the carbon .

There is no gelcoat just infused resin finish

Is there a special way I have to prime this for painting ???

Any info would be good on painting these panels

Im using two pack paint,,

Thanks Daz.
Reply
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
Cheers Rob ,

I thought I may need some special primer,,