Hanaldo
|
|
|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Without affecting the strength of the cure?
|
|
|
|
|
Dravis
|
|
|
Group: Forum Members
Posts: 592,
Visits: 1.9K
|
Just use the alcohol-type wood stain/dye powder... it works really well, and just a little will make the resin with filler a solid black.
"Sapere Aude"... Dare to KNOW! The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind... 103% of all people do not understand statistics... Do not adjust our mind, theres a fault in reality :-)
|
|
|
|
|
Hanaldo
|
|
|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I use fumed silica and calcium carbonate generally. Will try graphite powder as well and was thinking about getting some ground carbon fibre. I only mix by hand, haven't tried machine mixing.
|
|
|
|
|
brainfart
|
|
|
Group: Forum Members
Posts: 198,
Visits: 1.4K
|
> Plaster paddle mixer and a drill would mix it pretty thoroughly for larger batches
This will work ok for some fillers but unfortunately it will not properly disperse all additives or pigments.
|
|
|
|
|
ajb100
|
|
|
Group: Forum Members
Posts: 346,
Visits: 4.4K
|
Plaster paddle mixer and a drill would mix it pretty thoroughly for larger batches
|
|
|
|
|
brainfart
|
|
|
Group: Forum Members
Posts: 198,
Visits: 1.4K
|
What kind of fillers do you add, and what kind of black pigment have you tried? And how do you incorporate these into the resin? Stirring by hand or with a machine? Deep black is usually made with some kind of carbon black pigment. Obviously there are uncountable different commercial grades for many different applications available. If you buy black pigment pastes they are already diluted and you have no idea how much carbon is actually in there. Some might contain a lot and others just barely enough. A common ingredient for gelcoats and other resin mixtures is fumed silica thixotropy agent. This will work when mixed in by hand, but much less is required when high-shear mixers are used. Much less means 80 or 90% less in this case! Other fillers might behave similarly. So you can reduce the amount of filler materials by extremely intense stirring. Less white fillers and properly dispersed pigment means darker colour. This of course requires specialized equipment that is not available in your average hardware store.
|
|
|
|
|
Hanaldo
|
|
|
Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Yeh spot on with the that ajb, thanks for the reply Matt I am going to try adding some graphite powder into my next batch, this might give me a darker colour. Unfortunately I guess it just might not be possible to achieve a solid black when mixing my own gelcoats like this, though I'd be interested to hear what additives are used in professional gelcoats to give these properties without making them grey.
|
|
|
|
|
ajb100
|
|
|
Group: Forum Members
Posts: 346,
Visits: 4.4K
|
I tried reporting all the adverts but they all bounced back to my email address saying the server didn't like my email address
|
|
|
|
|
Matthieu Libeert
|
|
|
Group: Forum Members
Posts: 955,
Visits: 3.4K
|
Ok, Now I get the problem! never used some fillers and so on, so here stops my advice I think
|
|
|
|
|
Devin Wang
|
|
|
Group: Awaiting Activation
Posts: 4,
Visits: 28
|
Dear All,we can supply Gelcoat resin and pigment,we are manufacturer from China. Look at my signature.
Hey All: Do you want to import FIBERGLASS & RESIN from China? we are your NO.1 choice. This is Devin Wang from China CNBM(China National Building Material Corporation),a national owned company,14 years experience in the FRP material manufacturing.Our group owns more than 40 factories manufactured FRP material(fiberglass & Resin) through out China. 1)FIBERGLASS - E-glass fiber direct roving                      - Fob Shanghai USD 760/Metric Ton    
- E-glass fiber gun roving                         - Fob Shanghai USD 1060/Metric Ton
- E-glass fiber Chopped Strand Mat(powder &emulsion)         - Fob Shanghai USD 1330/Metric Ton
- E-glass fiber Woven Roving                   - Fob Shanghai USD 960/Metric Ton
2)RESIN - Unsaturated Ployester Resin(including Gelcoat resin,Vinyl Ester resin)
- Epoxy Resin
As to Resin price,we need your specification to confirm the prices. Welcome to inquiry! Best Regards, Devin Wang/Sales Manager CNBM/Composite Material Dept.
Address:Floor 17th, No.4 Building, Zhuyu International Commercial Center, No.9, Shouti South Road,Haidian District, Beijing 100048, China Tel:+86-519-83982873 Mobile:+86-13584510068 Fax:+86-519-83982891 E-mail:devinwang@okorder.com Website:www.icnbm.com,www.okorder.com
|
|
|
|