Talk Composites - The Forum for Advanced Composites

Pigmenting filled resins

http://www.talkcomposites.com/Topic11085.aspx

By Hanaldo - 5/5/2014 6:43:34 AM

Hey all,

Due to a lack of any available epoxy tooling gelcoats where I live, I have started making my own using laminating resin and a variety of fillers and additives. I like to add a black pigment, as the black makes it really easy to find low spots and polish to a great shine, however my issue is that most of the fillers I use are a white powder, so instead of a nice solid black gelcoat I end up with a sort of gunmetal grey. 

I have managed to get away with using that colour, but I would like to find out if it is possible for me to create my gelcoats with the solid black that I'm after. I don't want to add too much pigment obviously, and anything beyond 2% doesn't seem to do much regardless. So, how do proper tooling gelcoats like the Unimould system obtain such a nice black colour?
By Hanaldo - 5/8/2014 10:45:37 PM

Without affecting the strength of the cure?