Wooden Mold painting suggestion for Carbon Fiber Parts
Wooden Mold painting suggestion for Carbon Fiber Parts
Post Reply
Like
3
Wooden Mold painting suggestion for Carbon Fiber Parts
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Evripidis
Evripidis
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 23
Hi,
I m going to use wooden molds made of MDF and i would like to know what kind of color/primer should i use
to make carbon parts with safety. I made a test with cheap spray color and primer but it did not work. The result was
some color transfer in the carbon part from the mold. Could you suggest me something?
Thanks in advance
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Wooden Mold painting suggestion for Carbon Fiber Parts
Evripidis
-
11 Years Ago
You will need to use a 2k paint system, rattle cans wont be up to it. I'd use a 2k primer and a...
FLD
-
11 Years Ago
what FLD says is correct!
matthieutje65
-
11 Years Ago
If you can't spray 2k primer you can use these....
Brian_s
-
11 Years Ago
I concur with all the advice given. The paints are ideal when the surface is already dimensionally...
Warren (Staff)
-
11 Years Ago
Thank you all for the tips!!
Evripidis
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search