I concur with all the advice given. The paints are ideal when the surface is already dimensionally perfect for the part. Pattern-Coat Primer and Hi-gloss are better when an extra mm or so isnt a problem or the surface isn't as fine as you want.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|