By Evripidis - 5/3/2014 9:41:56 PM

Hi,

I m going to use wooden molds made of MDF and i would like to know what kind of color/primer should i use 
to make carbon parts with safety. I made a test with cheap spray color and primer but it did not work. The result was 
some color transfer in the carbon part from the mold. Could you suggest me something? 

Thanks in advance
By Evripidis - 5/7/2014 8:18:28 PM

Thank you all for the tips!!