Group: Forum Members
Posts: 468,
Visits: 2.7K
|
I've tried this! You can do it by overlapping but you get a dark line down the join where there's a step. Its not at all bad (1mm ish) but its there non the less. I think accepting this is far easier than butt jointing cloth. That would be a challenge! Overlapping 200g twill gives a much better result.
|