stalex
stalex
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 7
hello,
i am a new guy here and at the world of carbons!i want to create a laptop base from carbon ( i need it and i found it easy for first try). my problem is which materials i need to use to create the surface that i need for to do resin infusion and how to use these. the mold that i have is from wood . i think the surface from this video (
https://www.youtube.com/watch?v=VodfQcrXpxc
) is that i need. i tried to find the right kit to bought but i couldn't make it...
thank you for your time and any help will be welcome!
Tags
mold
surface
Reply
Like
7
Replies
stalex
stalex
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 4,
Visits: 7
first of all thank for help ! for some reason i can't see the picture that you sent me.i want to seal my mold , i want to create the right surface before i put carbon . my mold constructed on cnc !
Reply
Like
6
wozza
wozza
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
stalex (14/04/2014)
first of all thank for help ! for some reason i can't see the picture that you sent me.i want to seal my mold , i want to create the right surface before i put carbon . my mold constructed on cnc !
Hi, not sure why the link doesn't work. The product is from Easy Composites and is on their website under Mould Making materials, it is the Epoxy Mould Making Kit.
A picture of the "mould" will help as I am still not sure if you are describing the "mould" or the "pattern". Either way if it has been CNC machined from wood then the grain will need sealing. Epoxy coating resin may be suitable but more information would help.
Warren
Carbon
Copies Ltd
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
new guy!! help with mold!
stalex
-
12 Years Ago
https://www.easycomposites.co.uk/epoxy-mould-making-starter-kit This is the product used in the...
wozza
-
12 Years Ago
first of all thank for help ! for some reason i can't see the picture that you sent me.i want to...
stalex
-
12 Years Ago
[quote][b]stalex (14/04/2014)[/b][hr]first of all thank for help ! for some reason i can't see the...
wozza
-
12 Years Ago
This is the link: https://www.easycomposites.co.uk/epoxy-mould-making-starter-kit
Warren (Staff)
-
12 Years Ago
Don't know why your link bounced. Pictures of the mould would greatly help avoid confusion.
Warren (Staff)
-
12 Years Ago
i think the problem is that i don't speak very well english ! i will make one easy question ! in...
stalex
-
12 Years Ago
[quote][b]stalex (18/04/2014)[/b][hr]i think the problem is that i don't speak very well english ! i...
wozza
-
12 Years Ago
you help a lot !!! my mould is from wood .what materials i need to create the green surface before i...
stalex
-
12 Years Ago
you will have to 2K spraypaint your wood and do some sanding and bring it to a high gloss to seal...
matthieutje65
-
12 Years Ago
You are only likely to have issues with conductivity if the casing of the laptop was live and the...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search