hello,
i am a new guy here and  at the world of carbons!i want to create a laptop base from carbon ( i need it and i found it easy for first try). my problem is which materials i need to use to create the surface that i need for to do resin infusion and how to use these. the mold that i have is from wood . i think the surface from this video ( https://www.youtube.com/watch?v=VodfQcrXpxc ) is that i need. i tried to find the right kit to bought but i couldn't make it...
thank you for your time and any help will be welcome!
By Warren (Staff) - 5/7/2014 3:47:57 PM

You are only likely to have issues with conductivity if the casing of the laptop was live and the raw fibres were exposed.  Even with processes like infusion and pre-preg, there is still a very thin layer of resin between the carbon fibre and the surface.  This would likely be increased by a layer of laquer that is likely to be on furniture.

The "farraday cage" effect is unlikely to be significant on a flat table unless it directly obscures the path between the router and laptop, even then plenty of reflection should keep a signal plenty strong enough.