G200
G200
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 9,
Visits: 192
Hi , just wondering if you can use the carbon aramid (
https://www.easycomposites.co.uk/188g-plain-weave-carbon-kevlar
) with polyester or vinylester resin or is it epoxy only?
Thanks
Tags
Carbon aramid polyester
Edited
12 Years Ago by
G200
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Using carbon aramid with polyester resin?
G200
-
12 Years Ago
Yes, you can use either of those resins
ajb100
-
12 Years Ago
Thanks, is there any differences/advantages between poly and vinyl? Iv only ever used epoxy, just...
G200
-
12 Years Ago
you can use polyester-resin but It would be to bad using such an expensive good material with a...
matthieutje65
-
12 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search