Hi , just wondering if you can use the carbon aramid ( https://www.easycomposites.co.uk/188g-plain-weave-carbon-kevlar ) with polyester or vinylester resin or is it epoxy only?
Thanks
Edited 12 Years Ago by G200
ajb100
ajb100
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Yes, you can use either of those resins 
G200
G200
Supreme Being (199 reputation)Supreme Being (199 reputation)Supreme Being (199 reputation)Supreme Being (199 reputation)Supreme Being (199 reputation)Supreme Being (199 reputation)Supreme Being (199 reputation)Supreme Being (199 reputation)Supreme Being (199 reputation)
Group: Awaiting Activation
Posts: 9, Visits: 192
Thanks, is there any differences/advantages between poly and vinyl? Iv only ever used epoxy, just going for a cheaper option with this project
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
you can use polyester-resin but It would be to bad using such an expensive good material with a cheaper read weaker resin-type.

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com