Imperfect surface finish on resin infused part
Imperfect surface finish on resin infused part
Post Reply
Like
5
Imperfect surface finish on resin infused part
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
wpackham
wpackham
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 6,
Visits: 35
Guys,
I have just de moulded my 2nd resin infusion from the mould. The results are good, but not great.
My laminate consisted of three layers of carbon using the easycomposites infusion resin, peel ply and infusion mesh. The mould was treated with easylease and the part demoulded quite easily. The surface finish of the part appeared a little resin starved with consistent but very slight surface voids throughout the part surface.
I have actually achieved better results from vac bagging. Any suggestions why I'm not getting the perfect finish I was expecting? I had a full vacuum on the part throughout the infusion.
Advice would be appreciated.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Imperfect surface finish on resin infused part
wpackham
-
12 Years Ago
Some pictures of the problem areas would help. When you say you had full vac do you mean that the...
wozza
-
12 Years Ago
Hi Warren, Thanks for the reply. Having scoured the forum, I think I have determined the cause of...
wpackham
-
12 Years Ago
[quote][b]wpackham (10/03/2014)[/b][hr]Hi Warren, Thanks for the reply. Having scoured the forum,...
wozza
-
12 Years Ago
Thanks Warren, I'll try that tip on the next infusion. It's a steep and expensive learning curve!...
wpackham
-
12 Years Ago
[quote][b]wpackham (11/03/2014)[/b][hr]Thanks Warren, I'll try that tip on the next infusion. It's...
wozza
-
12 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search