Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
spray adhesive matt use for bonnet totorial
spray adhesive matt use for bonnet totorial
Post Reply
Like
2
spray adhesive matt use for bonnet totorial
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Edwin
Edwin
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 42
hi guys i cant find any of fibre adhesive in my place
can you guys help me out of this with other solution
or similar type of spray so i can use for my project
What is Spray No 1 that Matt is using??
can anyone explain it to me...what dose it do, what it is actualy
any similar brand i can use..for that
and so on spray No 2.. what dose it is where i can find it..
thanks guy. noob here lol.
Attachments
spray1.JPG
(
430 views,
74.00 KB
)
spray2.jpg
(
420 views,
95.00 KB
)
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
spray adhesive matt use for bonnet totorial
Edwin
-
11 Years Ago
Well the second spray is just acetone, that was used to activate the GC50 to make it tacky. As it...
Hanaldo
-
11 Years Ago
Hi Halando, thank for ur reply.. "Well the second spray is just acetone, that was used to activate...
Edwin
-
11 Years Ago
opss "hanaldo" heheh sorry spelling error
Edwin
-
11 Years Ago
You could try contacting 3M, see if they know someone in your area that stocks it? I thought I...
Hanaldo
-
11 Years Ago
spray glue like 'BISON' works fine to, don't know if its available where you live.
nickvancamp1
-
11 Years Ago
I have to reply to what Nickvancamp1 says... I wont say it's not true, might work, but this is the...
matthieutje65
-
11 Years Ago
I also had an issue with another brand of spray adhesive. It dissolved my release agent. Tried it...
Hanaldo
-
11 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search