Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I also had an issue with another brand of spray adhesive. It dissolved my release agent. Tried it twice with chemical release agent and wax, lost the part and mould both times. It was only the 3rd time that I tried PVA and then when I sprayed the adhesive I could visually watch it dissolve.
|