spray adhesive matt use for bonnet totorial


Author
Message
Edwin
Edwin
Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)Forum Member (48 reputation)
Group: Forum Members
Posts: 8, Visits: 42
hi guys i cant find any of fibre adhesive in my place
can you guys help me out of this with other solution
or similar type of spray so i can use for my project

What is Spray No 1 that Matt is using??
can anyone explain it to me...what dose it do, what it is actualy
any similar brand i can use..for that
and so on spray No 2.. what dose it is where i can find it..
thanks guy. noob here lol.
Attachments
spray1.JPG (418 views, 74.00 KB)
spray2.jpg (408 views, 95.00 KB)
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I also had an issue with another brand of spray adhesive. It dissolved my release agent. Tried it twice with chemical release agent and wax, lost the part and mould both times. It was only the 3rd time that I tried PVA and then when I sprayed the adhesive I could visually watch it dissolve. 