I am new to the composite repair process but have been playing around with different products and repairs.

My present situation is that I have been trying to repair a composite hockey stick that has broken in the shaft. I have tried a couple of techniques with both being unsuccessful. I have tried the repair from the inside using a carbon fiber sleeve and resin. It holds up but definetly not strong enough for a game of hockey and eventually breaks where the repair was done.

I have also tried on the outside, which lasted longer, but it eventually broke where the repair occurred. I believe I am either using the wrong type of sleeve or I a missing something in trying to do the repair.

If someone has some expertise or suggestions of what to use it would be greatly appreciated. I know it can be done.

Thanks for your help

Laroo
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I've made a little tutorial a while ago on how you could fix that problem...
This is more of a way of how I did it but like said above there are many ways solving that problem! 
Hope this might give you an idea 

I'd completely agree with the way of working of Warren!

PART1
 PART2

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search