I am new to the composite repair process but have been playing around with different products and repairs.
My present situation is that I have been trying to repair a composite hockey stick that has broken in the shaft. I have tried a couple of techniques with both being unsuccessful. I have tried the repair from the inside using a carbon fiber sleeve and resin. It holds up but definetly not strong enough for a game of hockey and eventually breaks where the repair was done.
I have also tried on the outside, which lasted longer, but it eventually broke where the repair occurred. I believe I am either using the wrong type of sleeve or I a missing something in trying to do the repair.
If someone has some expertise or suggestions of what to use it would be greatly appreciated. I know it can be done.
Thanks for your help
Laroo
|