Hi,posted this on the general composites...thought it might suit better here.

Hi
Id like to know what are the main differences between using a venturi vacuum system and a pump sistem.
Purchasing a venturi one seems cheaper(already have a good compresor),but Id like to know what is the downside if there is,and its limits.
We are focusing on small bycicle parts,no infusion.
Thanks in advance.
Replies
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
A Venturi will not produce the required vacuum, and is impractical to use for the hours needed
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
and they can be quite noisy