By udog - 2/20/2014 4:17:14 PM
Hi,posted this on the general composites...thought it might suit better here.
Hi Id like to know what are the main differences between using a venturi vacuum system and a pump sistem. Purchasing a venturi one seems cheaper(already have a good compresor),but Id like to know what is the downside if there is,and its limits. We are focusing on small bycicle parts,no infusion. Thanks in advance.
|
By udog - 2/21/2014 8:53:15 AM
Thanks for the replies OK,I understand that the ideal is a vacuum pump.Actualy,its what Im using now.I have an ole vacuum pump,that works.But I use it in my studio for degassing mostly silicone and some resins.Its a must for my daily job,and degassing only requires some minutes work for the pump in my case,and I dont like having it on for long periods. So,the next purchase will be a dedicated pump for Cbf,as recomended above.Also,now we are playing around with small parts,but who knows what will come after.For what I read the venturi might be a bit on the short side I guess. Thanks for claifying.
|
|