Carbon roof for Hummer 1


Author
Message
combustioncraig
combustioncraig
Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)Supreme Being (224 reputation)
Group: Forum Members
Posts: 26, Visits: 46
I am super impressed that is a huge job.  Good luck I am very interested to see how everything turns out 
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
Я благодарю за поддержку. Теперь я буду немного описать технический процесс, который был бы ясно, что к чему и сколько. 
http://s9.uploads.ru/t/1SzAu.jpg
Edited 11 Years Ago by shmat_ok (Nikolay)
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
http://s8.uploads.ru/t/cmudZ.jpg
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
http://s9.uploads.ru/t/h736y.jpg
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
Он решил использовать многослойную структуру исполнении крыше и крышку багажника. Арамида соты 10/3, толщиной 2 мм были для этой цели выбрали. Внешний декоративный слой ткани берется TR 50S 15K углеродного волокна 165г м2. Два последующее 0/90 и = 45/-45 12K TR50S углеродного волокна 650 г м2.http://s9.uploads.ru/t/pVKuR.jpg
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
These 3 layers ate about 3 kg of resin SR 8100/SD 8822 http://s9.uploads.ru/t/rkwZH.jpg
Edited 11 Years Ago by shmat_ok (Nikolay)
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
http://s9.uploads.ru/t/jycLz.jpg
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
http://s9.uploads.ru/t/LWzEd.jpg
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
http://s9.uploads.ru/t/SJFx5.jpgeverything sealed one more layer of C650t2 impregnated from above without vacuum, and placed in a vacuum bag for gluing together.
Edited 11 Years Ago by shmat_ok (Nikolay)
shmat_ok (Nikolay)
shmat_ok (Nikolay)
Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)Supreme Being (673 reputation)
Group: Forum Members
Posts: 101, Visits: 459
http://s8.uploads.ru/5QhrE.jpg