6/2/2013 5:51:41 PM
Hi, everybody! In this section I want to tell about the project over simplification of H1.
First I want to express special gratitude of Mr.Matt for video lessons at which I in principle and was trained in this business. Thanks.
Certainly at the beginning of the project I didn't think to keep the photoreport,
nevertheless it for me won't make special work. There are no photos with preparation of a surface for matrix removal so I will begin with a process half.
Also I am sorry for my English)
By felluco
-
3/10/2014 9:49:07 PM
wow
and many many kilograms of epoxy resin
Really ,very intersting work guys!