Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
If the resin is securely still in place, then the best way is to bleed resin into the cracks to hide the cracks. You may need to flex the splitter slightly to tease open the cracks and inject resin with say a cocktail stick or a syringe. Allow it go proud, then when cured sand back and polish back to even with surrounding surface.
Worst case you may need to sand right back on the resin to just before the cloth (with great care!!!) then fill with fresh resin proud of the hole and again when cured, sand back and flat to match surface.