for me the ooa of easy composites is perfect, nice tack on the surface of the mould...by having it that way it wont lift when adding the layers on top of that...did some test with a prepreg with less tack and I got annoyed while working with it, each time I've added a layer and tried to press it down, it got away from the surface of the mould

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
One more question since I have not worked with prepregs,

What level of "tack" is preferable? I'm would assume it is somewhat dependent of the intricacies of the tool but would you give some idea of a good handling level of tack? Is too much problematic is too little lead to distorition/movement of the stack?
THanks
20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
Thanks morepower, I had resorted to spamming every prepreg company on this continent asking whether they have ooa suitable materials etc... 

Will look into cytec
morepower
morepower
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
Try Cytec. They should have VTF261 in stock... It may be made in the UK but I would bet they have stock in the USA as it is a US based company. 

https://www.cytec.com/
20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
Ya google gets me nowhere with that. I have contacted tencate about their OOA prepreg

I would be open to use the easycomposites but being so far, shipping will likely be a pain and the time it takes to ship would be long too.... 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
you can find some prepreg on www.easycomposites.co.uk 
Because I live in europe I order there, don't know about buying it in the US or canada, just do a quick search on google I guess?! Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
http://www.ambercomposites.com/prepreg/out-of-autoclave-prepreg/

anyone have any experience with this?

I live in Canada and I'm having a hard time tracking down any OOA materials. Anyone have suggestions for anything in Canada or the USA? Alternatively I might have to bit the bullet and buy from somewhere in Europe....

Any other sources would be appreciated. 

Until now I've been doing infusions but I'm really tired of the whole infusion process and need a change. Its a PITA with the whole layup and then the trimming afterward. Prepreg might just let me cut back on the amount of post production trimming....