I want to attach this to a small hook and was thinking a knot would work with many other materials but maybe impossible or inadvisable with this product. If possible, what knot would you recommend?
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I wouldnt recommend a knot as it would likely snap.

It is quite a small part to bond to, but bonding would be your best solution. You may need to fabricate a bonding surface on the hook so you can bond over a decent length of rod.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant