Vacuum bagging when skinning


Author
Message
redrumredrum89
redrumredrum89
Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)Forum Guru (62 reputation)
Group: Forum Members
Posts: 8, Visits: 77
Can you use any kind of vacuum bagging Technic for skinning ?  Thanks 
Reply
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
It will work and if you work with a stretchable bagging material it will give you a good finish straight from the bag.
About putting it in place: add some resin, let it go to a tacky state place the carbon, wet the carbon, add bag and done Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search