Can anybody point me to epoxy resin system that does not use a yellow-ish hardener? Possibly something more neutral like blue or something? I am using an amazing epoxy resin system from a German company, but the hardener is yellow and in bright sunlight, you can see the yellow tint on the infused things....Anybody got a clue? Possibly a pigment that I can put in the hardener? I know Koenigsegg uses some kind of pigment to tint the resin to whatever color they want but still keep it transparent...
Reply
StanTheMan
StanTheMan
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 61, Visits: 380
matthieutje65 (17/12/2013)
Are you looking for pigments or a totally transparent epoxy A+B? by adding white it will get worse than the yellow-ish kind of look you have right now


No, no, I still want to keep the transparency. The pigment part was in case all hardeners out there are yellow. What I'm really looking for is a non-yellow hardener. Are all epoxy hardeners yellow-ish?