hey guys,
This is my first post so I hope I'm doing it right 

I have the idea of making a Siliconevacuumbag myself... I don't know if I'm extremely optimistic?!
this is the plan: 1.Put the finished car bag in its mould
                         2.Tape of the edges so that the resin can not flow between the part and the mold
                         3.laying up the exit and insert for the vacuum and tubes
                         4.brushing a thin layer of transparent silicone onto everything
                         5.let it cure for a while and wait till it get tacky
                         5.put some reinforcementmesh on it
                         6.brush a new thin layer of silicone above the reinforcement
                         7. let it cure and remove
 
 
ps: I've used peelply on the inside of the car so there is a pattern on the inside that could maybe replace the infusionmesh?!
does this sound like plausible? or am I missing something?
If interested for the making of this model of the car check out the youtubevideo
https://www.youtube.com/watch?v=0tosbURJY0Q&feature=plcp&context=C3b08128UDOEgsToPDskKeK8cmT-KGOiUJQZ4T4WWQkind regards Matthieu Libeert                
			            				
			            
Matthieu Libeert
Founder MAT2 Composites X Sports
website: www.mat2composites.com