hey guys,

This is my first post so I hope I'm doing it right Whistling

I have the idea of making a Siliconevacuumbag myself... I don't know if I'm extremely optimistic?!

this is the plan: 1.Put the finished car bag in its mould

                         2.Tape of the edges so that the resin can not flow between the part and the mold

                         3.laying up the exit and insert for the vacuum and tubes

                         4.brushing a thin layer of transparent silicone onto everything

                         5.let it cure for a while and wait till it get tacky

                         5.put some reinforcementmesh on it

                         6.brush a new thin layer of silicone above the reinforcement

                         7. let it cure and remove

  

ps: I've used peelply on the inside of the car so there is a pattern on the inside that could maybe replace the infusionmesh?!

does this sound like plausible? or am I missing something?

If interested for the making of this model of the car check out the youtubevideo

https://www.youtube.com/watch?v=0tosbURJY0Q&feature=plcp&context=C3b08128UDOEgsToPDskKeK8cmT-KGOiUJQZ4T4WWQ

kind regards Matthieu Libeert

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search