Hey Jap,

They say its lasercut.

The part need to be cured to be cut.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
japcarmaniac
japcarmaniac
Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)Supreme Being (401 reputation)
Group: Forum Members
Posts: 53, Visits: 157
didnt see that the first time lol. would it be possible to wet out some carbon fibre, leave it to cure a little the trim it with a scalpel then sandwich it between two hard smooth surfaces to fully cure?


Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Not sure if you can Lasercut Carbonfiber?! would more likely to be CNC-milled... but not sure

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
I would rather use watercutting or as you mentioned, cnc milling. But cnc milling a flat plate like this would need a vacuum table to make all cuts at once.

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search