By japcarmaniac
-
2/27/2012 6:35:18 PM
http://www.ebay.co.uk/itm/BMW-3-SERIES-E46-Real-Carbon-Fibre-Interior-Dial-Surrounds-318i-320i-325i-330-/320805268924?pt=UK_CarsParts_Vehicles_CarParts_SM&hash=item4ab17bedbc#ht_2370wt_1187
are they cut out when its still slightly soft?
By Joe
-
2/28/2012 4:13:48 PM
I would rather use watercutting or as you mentioned, cnc milling. But cnc milling a flat plate like this would need a vacuum table to make all cuts at once.