I've been gathering stuff now. And finally I'm ready to just do this. 

I've got my plug ready. Got my resin, glass and picked up some graphite powder for surface coat. 

I really didn't think about this till now but I've got no way to measure my resin. Would a paint mix cup such as one from harbor freight work?

How much graphite to resin should be used?
My resin is wb400 with LH101 hardner from resin services. 

Thos project is really small in size. It's a knife handle. The  mold will be a 2piece as there is no way to bag in between I will make the 2 sides and bond them together using the molds. 

I have access to a vacuum pump but I don't have any real vacuum bag material. I'm gonna attempt to use a space saver bag. I'm running a test to see if the vacuum last overnight. 
As I remember it held well in it's intended purpose. 

I've got some polyester batting for breather, I'm planning on plastic wrap for release film. 



I guess I'm just looking for some confirmation that yeah everything sounds ok, not the best but good enough for a garage one time deal. 

Thanks. 
Replies
carbonBullet
carbonBullet
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 60
Well. First half of mold is finished. 

I ended up with 1gram graphite to 5 grams resin. Probably a little high but worked for me. 

Big issue is my plug broke on removal. So repair jas to be done. 

I have one little chip on and egde. It was from not cleaning the surface coat out of the edge there. 

Mental note: do not use those space bag things, total junk. The actual plastic leaked. 

I used a wonderful white trash bag, and electrical tape. Freaking awesome. 

One othe mental note, you must poke holes in your release film, in my case plastic wrap. That's ultimately what broke my plug resin bleed on the opposite side. 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Those space saving bag CAN work, I always use them, even with prepreg carbonfiber at high temparatures +100°C the bag keeps a full vacuum with vacuumpump shut down for more than 2 days, maybe try to find better ones? Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search