Those space saving bag CAN work, I always use them, even with prepreg carbonfiber at high temparatures +100°C the bag keeps a full vacuum with vacuumpump shut down for more than 2 days, maybe try to find better ones? Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




carbonBullet
carbonBullet
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 60
Well. First half of mold is finished. 

I ended up with 1gram graphite to 5 grams resin. Probably a little high but worked for me. 

Big issue is my plug broke on removal. So repair jas to be done. 

I have one little chip on and egde. It was from not cleaning the surface coat out of the edge there. 

Mental note: do not use those space bag things, total junk. The actual plastic leaked. 

I used a wonderful white trash bag, and electrical tape. Freaking awesome. 

One othe mental note, you must poke holes in your release film, in my case plastic wrap. That's ultimately what broke my plug resin bleed on the opposite side. 
carbonBullet
carbonBullet
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 60
Thank you Chris.
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
EC state 10% by weight ( EC product ) so i would use this as a starting point.
Regards Chris
www.carbonfibrewoks.co.uk

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
carbonBullet
carbonBullet
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 60
I know, I should not skimp on bagging.  But money and mostly lack of time is killing me.  I can't buy any 'real' bagging materials local, I've got only this weekend for this project and I'm out of money for now.  So it's all or nothing....

can someone tell me about how much graphite powder to resin should be used.  The graphite I picked up from a tractor supply store a whole large can of it was only 6$....nice find if you ask me...
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
If cash is tight remember to stock up on McDonald's wooden coffee stirring sticks Wink
Chris
www.carbonfibreworks.co.uk   

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
wojtepanik
wojtepanik
Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)Supreme Being (755 reputation)
Group: Forum Members
Posts: 102, Visits: 582
Hi,
If you want to cut the coasts you can always use thick garbage bag, and seal it with some bathroom silicone and zip ties.   but this way sucks. Invest 30 £ more and get proper vacuum stuff. Trust me you can ruin your part if for ex. Your bag will not be stretchy enough it could be torn apart by the vacuum. You don't have to use perforated film or breather cloth, cheap peel ply and toilet paper will do the job. I would never replace bagging film and bagging tape with some cheap s***, all your work depends on that. if you are creative you can make your bag reusable as you prepare special seal for that ,that's how I do with most of my bags. 
Bye 
Wojtek from Poland

~~~Everytime I hear sound of demoulding part I have eargasm~~~
carbonBullet
carbonBullet
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 60
I found a decent digital scale at harbor freight.  so my measure issue is cleared.

I have also found the vacuum storage bag not to be ideal, it does hold but not real good, so it's not a nice vacuum.  I have some aluminum tape so I may attempt to cut one in half and seal it with tape, possibly making a better seal.

I also picked up a space heater to work in my garage. 
carbonBullet
carbonBullet
Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)Forum Member (40 reputation)
Group: Forum Members
Posts: 6, Visits: 60
I'm not using polyester resin. It's epoxy. So it really needs to be close as I can get it. 

What about the powder. How much you think?
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Tbh, I use plastic cups from morrisons as mixing cups, they're inexpensive and throw away after use. For something that size, you'll probably need a set of jewellery scales which to hundreds of a gram, although you can't go too far wrong with polyester