I´m trying to replicate a wing but i´m having hard times figuring how can i do the seams of the top and bottom part so i can have a good cosmetic finish.
The problem is the seams on the original wing are in the angles (V shaped) so i can find out how i will make a flange in the two sides were i can aply the bonding agent.

Here are some photos to illustrate

http://i41.tinypic.com/2h6dnvn.jpg
http://i41.tinypic.com/ih61wh.jpg
http://i44.tinypic.com/16706qb.jpg






Any help would be much appreciated

Thanks in advance
Replies
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Oooops. Reading the original post again I think you may be right FLD.

I do very similar to you except I use 3mm Soric in the lay-up around the split line on the leading edge. When trimmed this gives a 4mm wide edge to bond the two halves together. So don't need the tape along the join.

Warren

Carbon Copies Ltd
Edited 12 Years Ago by wozza
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
wozza (25/11/2013)


 I use 3mm Soric in the lay-up around the split line on the leading edge. When trimmed this gives a 4mm wide edge to bond the two halves together. So don't need the tape along the join.

Warren


Very good idea! Wish I'd heard that/thought of that sooner!