Hi! My customer wants to replace his sliding sunroof with cf flat sheet. He wants it to be quiet stiff but light. I have 3mm soric-like core material, 220gsm cf, 200gsm diolen, wide variety of woven glass clothes and some uni-dir cf 200g 5cm wide cf tape. I could use poly resin as it is uv stable, but I have epoxy also. It will be mounted with rivets to the roof. These are the dimensions : 40cmx80cm or 16inx32 in. How do you suggest to make my layup? I thought about poly resin and carbon/diolen/about 300gsm glass/core/300gsm glass/ cf or diolen. It is for racing purpose.I will laminate it on piece of glass. Please share your suggestions and experience. Thanks for taking your time reading that! Bye Wojtek from Poland