Hi folks, As the winter is here now what is the lowest recommended curing temp for EL2 & IN2.
It is currently dropping down to 6degC here in my shed and I was wondering if the resin will eventually cure at this temp?
Kind regards,
aran01
Reply
baja_patient
baja_patient
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Can you heat the shed? How can you work in 6 degrees anyway? Alternatively, find a place to work inside the house.

cheers