Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Resins, Gelcoats and Pigments
»
curing temp
curing temp
Post Reply
Like
1
curing temp
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
aran01
aran01
posted 11 Years Ago
ANSWER
Topic Details
Group: Forum Members
Posts: 8,
Visits: 30
Hi folks, As the winter is here now what is the lowest recommended curing temp for EL2 & IN2.
It is currently dropping down to 6degC here in my shed and I was wondering if the resin will eventually cure at this temp?
Kind regards,
aran01
Reply
Like
1
Reply
ajb100
ajb100
posted 11 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
What unused to do before getting my workshop sorted was infuse outside in the cold, then clamp the lines, cut them off as close to the clamps as possible and then put it in the airing cupboard under a duvet with the hot water on for an hour.
With the water on it would reach 40 deg then stay warm all night, easily warm enough to cure fully. As its in a sealed vac bag, there's no smell etc
For larger projects, I used an electric blanket under a large duvet to keep it warm
Reply
Like
1
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
curing temp
aran01
-
11 Years Ago
You MUST keep it around 20C if you want a successful cure. if you are lucky you might get away with...
Warren (Staff)
-
11 Years Ago
What unused to do before getting my workshop sorted was infuse outside in the cold, then clamp the...
ajb100
-
11 Years Ago
Can you heat the shed? How can you work in 6 degrees anyway? Alternatively, find a place to work...
baja_patient
-
11 Years Ago
Build a warm box for your resin and cloth, doesn't need to be much just an MDF box with a low...
ChrisR
-
11 Years Ago
Thanks guys for the feedback. I am working with a heater but I am moving the parts indoors once...
aran01
-
11 Years Ago
Last winter I made some parts that latterly 1mth later still hadn't cured... I found if it didn't...
andygtt
-
11 Years Ago
Like everyone says, don't make parts under 15°C or I would even say 20°C as a small remark I would...
matthieutje65
-
11 Years Ago
[quote][b]andygtt (21/11/2013)[/b][hr]Last winter I made some parts that latterly 1mth later still...
stuart321
-
11 Years Ago
Post Reply
Like
1
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search