car paint under coating resin?


Author
Message
benet
benet
Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)
Group: Forum Members
Posts: 59, Visits: 373
I finish of  parts with a layer of coating resin applied to a cured and sanded part. could i paint the part with a spray can ( car paint ?) then sand and coat with coating resin and get a good result?

if so do i need a specific type of paint.

I do not have a compressor etc.

thanks

ben
wojtepanik
wojtepanik
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 102, Visits: 582
So you want to have the best finish ? Glossy etc? The best way is to coat part with resin, then sand smooth and spray automotive can clearcoat 

~~~Everytime I hear sound of demoulding part I have eargasm~~~
benet
benet
Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)Supreme Being (897 reputation)
Group: Forum Members
Posts: 59, Visits: 373
wojtepanik (20/10/2013)
So you want to have the best finish ? Glossy etc? The best way is to coat part with resin, then sand smooth and spray automotive can clearcoat 


No, i want a painted design under the coating resin. In the past i have only coated onto wood or carbon or cloth but never onto  a painted surface, will it work , what paints are good what to avoid ?
wojtepanik
wojtepanik
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 102, Visits: 582
I see, so best way to do it is to paint your pattern on the cured element and then coat it again with resin or some clearcoat 

~~~Everytime I hear sound of demoulding part I have eargasm~~~
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
It should work by painting it and then coat it with a coating resin... but a good hint I can give you is test it out on a scrap-part before doing the real job.
I've seen some spraypaints reacting with an epoxyresin (causing the spraypaint to bubble)

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




baja_patient
baja_patient
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 135, Visits: 1.6K
Yeah dont think you should coat those normal spray can paints...

Might get unwanted results.

If it is a "normal" RAL color, you could just put some pigment in your coating resin, save yourself a lot of work. Then sand and polish.
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Matthieu is dead right.

Rattle can paints are loaded with solvants which can take months to fully go at room temperature. The solvants can react badly with resins.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
jarrenS
jarrenS
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 1, Visits: 2
There are a ton of things that individuals ignore and some of the most innocent things take a lot of work. Car paint, for example, has to undergo a lot of screening before it can get put on a car. Car paint testing involves exposing shades of paint to years of intense climate conditions to see if it can stand up. Article source: Car Paint Testing.
kidpaint
kidpaint
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 99, Visits: 676
i dont see why you couldnt just use an auto grade paint, paint it then use am auto clear over top of that? 
Matthieu Libeert
Matthieu Libeert
Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)Supreme Being (12K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
I've recently finished this video on my youtube-channel concerning clearcoating and so on, might be interesting for some of you!



Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search