Hi folks,
I am trying to do up a shopping list for a repair to a boat.
I need to make some panels to match what is currently there and I was wondering if anyone can provide a sizing guide on how many layers of Woven Glass 290g I would need to make a laminate 6mm thick?
Also how can I calculate how much resin 1sqm of this laminate at 6mm thick I need using infusion resin IN2?
Many thanks in advance.