Group: Forum Members
Posts: 156,
Visits: 14K
|
Another way to help is use a resin or hardener with a longer open time,when I infuse I use a harderner with a 3hour pot life which give me after mixing,15 to 20 minutes degasing time which depending on temperature usually give Krystal clear resin
|