It is also for cosmetic reasons. Probably a similar product to our GC50 or other polyester based clear gelcoats. The surface wouldnt necessarily be full of voids if laminated properly.
Could also be done to provide UV protection and some scrape protection for the carbon. A nice layer of gelcoat can have scratches sanded out where as with say an infused carbon panel, the layer of resin over the carbon is very thin and easy to wear through to.