Group: Forum Members
Posts: 10,
Visits: 132
I've visited a jet-ski factory and I saw that they spray a gelcoat(polyester) on tool surface before laminating the first layer.
Does anyone know why they need to gelcoat at first ? I thought gelcoat only use for mold making purpose.
and how is a different between this gelcoat and gelcoat which is used to make a mold ?
Please kindly to help.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Gelcoat application
kornpetpani
-
12 Years Ago
If you don't apply the gelcoat first, you will see the fibreglass, which is not very attractive....
carboncactus
-
12 Years Ago
The gelcoat I saw is transparent, I think because they need to show a CF feature on jet ski's...
kornpetpani
-
12 Years Ago
In that case, its because the surface will be full of voids otherwise.
carboncactus
-
12 Years Ago
If it just to protect a surface purpose, could I use normal epoxy resin instead of gel coat....
kornpetpani
-
12 Years Ago
It is also for cosmetic reasons. Probably a similar product to our GC50 or other polyester based...
Warren (Staff)
-
12 Years Ago
Thank you very big for your kindness help. How about your product CG50(polyester based gelcoat),...
kornpetpani
-
12 Years Ago
Hi, yes it is compatible with epoxy, but in my work, I don't use any topcoat/gelcoat I use only...
wojtepanik
-
12 Years Ago
Just like Warren said it gives you the possiblity to have some errors and fix them if...
matthieutje65
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search