tangotop
tangotop
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 11,
Visits: 148
I'm currently making a buck to make a mould for a diffuser. Based around a wooden construction with a fibre board to get a good curve. I am wondering what a good sealer for this would be.
The base board is MDF... having already taken a mould for another part using MDF as a base I know that this will not absorb the resin. However I do need to get a reasonable finish to this area on this occation/
I have seen on other forums that some people use Bonda G4 water seal... which isn't easy sourced. Are there other alternative such as a concrete seal? What have others used...
I also need to finish off the edges of the diffuser with a fillet or newplast before moulding commences so it will need to either go over or under this.
Edited
14 Years Ago by
tangotop
Reply
Like
6
Reply
Dave
Dave
posted 14 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 48,
Visits: 253
a slightly pointy spoon can be great for making variable fillets. Go in the direction of the back of the spoon (convex side). The angle you hold the spoon at changes the radius of the fillet
Dave.
Edited
14 Years Ago by
Dave
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Sealing a buck/plug
tangotop
-
14 Years Ago
Hi, Tango. I use polyester filler (2k) andit never disappointed me. It builds thickness fast, can...
Joe
-
14 Years Ago
ok... so i've now got the curve on and I've softened the edging with newplast. Can I still use...
tangotop
-
14 Years Ago
I know we've just spoken on the phone about this but I'll put the same reply on the forum so it...
Matt (Staff)
-
14 Years Ago
Maybea little cheap but useful tip to apply body-filler: Use a rubber rectangle that you fold so...
Joe
-
14 Years Ago
Thanks Guys... :) Will get cracking on this this weekend
tangotop
-
14 Years Ago
a slightly pointy spoon can be great for making variable fillets. Go in the direction of the back of...
Dave
-
14 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search