Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
Sealing a buck/plug
Sealing a buck/plug
Post Reply
Like
9
Sealing a buck/plug
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
tangotop
tangotop
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 11,
Visits: 148
I'm currently making a buck to make a mould for a diffuser. Based around a wooden construction with a fibre board to get a good curve. I am wondering what a good sealer for this would be.
The base board is MDF... having already taken a mould for another part using MDF as a base I know that this will not absorb the resin. However I do need to get a reasonable finish to this area on this occation/
I have seen on other forums that some people use Bonda G4 water seal... which isn't easy sourced. Are there other alternative such as a concrete seal? What have others used...
I also need to finish off the edges of the diffuser with a fillet or newplast before moulding commences so it will need to either go over or under this.
Edited
14 Years Ago by
tangotop
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Sealing a buck/plug
tangotop
-
14 Years Ago
Hi, Tango. I use polyester filler (2k) andit never disappointed me. It builds thickness fast, can...
Joe
-
14 Years Ago
ok... so i've now got the curve on and I've softened the edging with newplast. Can I still use...
tangotop
-
14 Years Ago
I know we've just spoken on the phone about this but I'll put the same reply on the forum so it...
Matt (Staff)
-
14 Years Ago
Maybea little cheap but useful tip to apply body-filler: Use a rubber rectangle that you fold so...
Joe
-
14 Years Ago
Thanks Guys... :) Will get cracking on this this weekend
tangotop
-
14 Years Ago
a slightly pointy spoon can be great for making variable fillets. Go in the direction of the back of...
Dave
-
14 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search