Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Can this shape be skinned with a single piece of fabric?
Can this shape be skinned with a single piece of fabric?
Post Reply
Like
3
Can this shape be skinned with a single piece of fabric?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 380
It's a fiat 500 mirror cap. I was wondering whether this kind of shape can be skinned with a single piece of carbon fiber fabric or I should do 2? I have the easycomposites ProFinish fabric. This is my second attempt so please bear with me
Attachments
photo 1.JPG
(
230 views,
94.00 KB
)
photo 2.JPG
(
200 views,
100.00 KB
)
photo 3.JPG
(
193 views,
90.00 KB
)
photo 4.JPG
(
194 views,
86.00 KB
)
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Can this shape be skinned with a single piece of fabric?
StanTheMan
-
12 Years Ago
Yes you'll do this with one piece quite easily. I did this with one piece which was also my first...
r0bsk1
-
12 Years Ago
Man, I'm either an idiot or can't do sh1t lol. I lay the dry fabric over the cap and I get wrinkles....
StanTheMan
-
12 Years Ago
[quote][b]StanTheMan (21/08/2013)[/b][hr]Man, I'm either an idiot or can't do sh1t lol. I lay the...
carbonfibreworks
-
12 Years Ago
[quote][b]carbonfibreworks (21/08/2013)[/b][hr][quote][b]StanTheMan (21/08/2013)[/b][hr]Man, I'm...
StanTheMan
-
12 Years Ago
Simple curve:...
carboncactus
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search